310 Stainless Steel because of its high content of chromium and nickel medium, resistance to oxidation corrosion at the minor cycle condition of up to 2000 ° F.310 has good resistance to heat and other forms of corrosion of sulfide corrosion and widely applied in the medium in the carburizing atmosphere.
such as petrochemical environment, such as more demanding industrial heat treatment furnace carburizing atmosphere needs to choose RA330 ® or RA333 ®.It is not recommended to use 310 in the thermal shock corrosion condition of the intense circulating liquid quenching.
310 Stainless Steel Sheet Plate Round Bar Tubes Chemical Composition | ||||||||||
| Cr | Ni | C | Si | M | P | S | Mo | Cu | Fe |
min | 24.0 | 19.0 | - | - | - | - | - | - | - | - |
max | 26.0 | 22.0 | 0.08 | 0.75* | 2.0 | 0.045 | 0.03 | 0.75 | 0.5 | Balance |
310 can provide different products form, its grain size and carbon content meet the 310 s and 310 h specification requirements, the strength of the excellent low temperature - 450 ° F, and low permeability, often used in low temperature environment, according to the evaluation of AISI B1112 machining performance of 42%.When using a high speed steel tool, process it at 70 feet/min. It is recommended to process it at room temperature and use AWS e310-15 electrode or ER310 welding wire.
Material standard: AMS 5521 EN 10095 UNS S31008.
Product form: 310 rolls, 310 plates, 310 welding products, 310 coil, 310 tubes, 310 tubes, 310 thin plates.
Physical Performance | |
Density | Melting Point |
0.284lb/inch3 | 2470-2555℃ |
Temperature, °F | 70 | 1000 | 1200 | 1400 | 1600 | 1800 | 2000 |
Coefficient of thermal expansion, in/in°F*10-6 | - | 9.5 | 9.8 | 10.05 | 10.15 | 10.3 | 10.6 |
Heat conductivity | 7.6 | 13.6 | 15.2 | 16.8 | 18.4 | 20.0 | - |
Elasticity modulus | 29.0 | 23.0 | 21.8 | 20.5 | 19.2 | - | - |
*70°F to indicated temperature.
310 Stainless Steel Characteristics:
Resistance to high temperature oxidation temperature of 2000 ° F moderate heat corrosion under low temperature strength and toughness.
Typical tensile property
Largest strength of extension, ksi | 10 | 1000 | 1200 | 1400 | 1600 |
0.2%yield strength, ksi | 80.0 | 67.8 | 54.1 | 35.1 | 19.1 |
Ductility,% | 35.0 | 20.8 | 20.7 | 19.3 | 12.2 |
HB,Brinell | 52 | 47 | 43 | 46 | 48 |
Typical creep fracture performance
>
Temperature, °F | 1200 | 1400 | 1600 | 1800 |
Smallest creep strength.ksi | 14.9 | 3.3 | 1.1 | 0.28 |
10,000 breaking strength, ksi | 14.4 | 4.5 | 1.5 | 0.66 |
310 Stainless Steel application:
fire the tip of the tongue of fluidized
bed coal combustion devices
radiant tube oil refining and cradle of the steam boiler
coal gasifier internal components
thermocouple
tank fire bolt burner
the combustion chamber furnace
muff
cupping food processing equipment
structure pieces at low temperature
Original package or neutral package.
According to clients’ needs.
Shipped in 10-35 days after payment.
Spot delivery, including delivering small batches of goods
Provide wide-range and complete materials series products
Cutting plates, including complex shapes of materials and special processing and disposal
Cutting bars and strips
Our application technology expert provide the best material and recommendation
One-stop service