Ferrite content is not greater than 0.6, especially for urea industry.
725 LN Stainless Steel Round Bar | |||||||
Chemical Composition | C | Si | Mn | P | S | Cr | Ti |
Standard | ≤0.03 | ≤1.00 | ≤1.00 | ≤0.045 | ≤0.22 | 17.0-18.5 | 0.2+(C+N)~1.0 |
General | 0.008 | 0.18 | 0.2 | 0.020 | 0.001 | 17.50 | 0.3 |
725LN Stainless Steel Characteristics:
ASTM UNS S31050 EN 1.4466 725LN Stainless Steel has High Ni and Mo austenitic grade with similar corrosion resistance to 904L. Typically used in Urea applications. Available as plate only.
Distinction | Mechanical Performance | |||
Ys(Mpa) | Ts(Mpa) | El(%) | Hv | |
Standard | ≥240 | ≥450 | ≥22 | - |
General | 290 | 430 | 32 | 150 |
725LN Stainless Steel Physical Performance | ||||
Density(g/cm3) | Magnetism | Specific heat | Heat conductivity 1000C(W/M.0C) | The coefficient of thermal expansion 20~1000C(10-6/0C) |
7.7 | Yes | 460 | 26.4 | 10.5 |
725LN Stainless Steel Application:
Urea applications
Pulp & Paper industry
Flue gas cleaning
Chemical industry
Pharmaceutical industry
Standard exporting package.
Original package or neutral package.
According to clients’ needs.
Shipped in 10-35 days after payment.
Price
Q: How can I get the price?
A: You can contact us through sending inquiry, or get price list by Email.
Delivery
Q: How long is the delivery time?
A: It depends on quantity. Usually, 10-35 working days.
Sample
Q: Can I get sample to check the quality?
A: Of course. We can supply sample, and free for some small value products.
OEM
Q: Do you provide OEM service?
A: Yes, we do. Customized design is available.
Payment
Q: What is your payment term?
A: L/C, T/T, Paypal, Western Union, etc.
Certificate
Q: What certificate do your products have?
A: CE, ISO9001, RoHS, SGS, etc.